Description
Fe-Ni-Co is ternary alloy three-partalloy, curie point up to 300℃. Low coefficient of expansion between -20~300℃, under the -60℃ austenite and martensite maintain the same. In the atmosphere, water and seawater has good corrosion resistance.
Application
Mainly used in the manufacture of requirements between -50 ~ 300℃, applied in high precision instrument parts and electronic device.
parameter
Typical chemistry:
C | Si | P | S | Mn |
Ni |
Co |
Fe |
≤ | |||||||
0.05 | 0.15 | 0.020 | 0.020 | 0.25 | 32.4-33.4 | 7.00-8.00 | Balance |
Physical property:
Heat Treatment of the Samples | Mean Coefficient of Linear Expansion | |
20~l00℃ | 20~300°C | |
To heat the semi-finished products samples to 840±10°C, hold for 1hour, and quench in the water. Machine the samples to finished samples. And heat at 315±10℃ for 1h, furnace or air cool. | ≤2.0 |
Typical Coefficient of linear expansion(/10-6K-1):
20~50℃ | 20~100℃ | 20~200℃ | 20~300℃ | 20~400℃ |
1.4 | 1.3 | 1.2 | 1.7 | 4.5 |
Size Range
Sheet | Thickness:0.10mm~3.50mm, width: ≤300mm |
Plate | Thickness:3.5mm~4.0mm, width: ≤300mm |
Round wire | Thickness:0.10mm~5.0mm |
Flat Wire | Dia 0.5mm~Dia 5.0mm, length≤1000 |
Rod | Dia 5.0mm~Dia 8.0mm, length≤2000 |
Dia 8.0mm~Dia 32.0mm, length≤2500 | |
Dia 32.0mm~Dia180.0mm, length≤1000 | |
Capillary | OD 8.0mm~1.0mm,ID 0.1~8.0 length≤2500 |
Pipe | OD 120mm~8.0mm,ID 8.0~129 length≤4000 |
Condition: (With max tolerance) cold rolled, cold drawn, hot rolled , hot forging ,peeled turned ,bright ,bright annealed