Description
Comolloy has good hysteresis characteristics in the high magnetic field.
Application
The main application of this alloy for whole hysteresis motor rotor.
parameter
Chemical Composition (%)
C | Si | P | S | Co | Mo | Mn | Fe |
≤ | |||||||
0.03 | 0.30 | 0.025 | 0.025 | 11.0~13.0 | 16.5~17.5 | 0.10~0.50 | Balance |
Magnetic Property
Magnetic field intensity(Hμ) | Oe | 300~360 |
Flux Density (Bμ) | T | 0.9~1.2 |
Pμ | erg/cm3≥ | 4.7×105 |
Kμ≥ | kμ≥ | 0.45 |
Size Range
Bar | Dia 8.0mm~Dia 32.0mm,length:≤3000mm |
Dia32.0mm~Dia150.0mm,length:≤1300mm |
Condition: (With max tolerance) hot rolled,bright,bright annealed,hot forging,peeled,turned,hot treated