Description
This is a kind of low Curie temperature (25 ℃ ~ 200 ℃) alloy, its outstanding characteristic is below the Curie temperature, magnetic induction intensity decreases sharply with the temperature rise, and is almost linear relationship.
Application
Permanent magnet of the traveling wave tube, magnetron,voltage regulator, mileage rate table, gas table, temperature, magnetic shunt compensation of watt-hour meter and other components or thermal components.
parameter
Cross Reference
IEC | Russia | U.S.A | Japan |
- | 30H | ThermoPerm | MS-1 |
Chemical Composition (%)
C | P | S | Mn | Si | Ni | Fe |
≤ | ||||||
0.04 | 0.020 | 0.020 | 0.40 | 0.30 | 29.5~30.5 | Balance |
Physical Property
Density(g/cm3) | 8.1 |
Magnetic Property
When magnetic field intensity is 8000A/m, the magnetic induction(B/T) at different temperatures B8000 | ||||
-20℃ | 20℃ | 40℃ | 60℃ | 80℃ |
0.40~0.60 | 0.20~0.45 | - | 0.02~0.13 | - |
Size Range
Sheet | Thickness: 0.05mm~0.50mm,width10.0~210.0mm |
Plate | Thickness: 3.5~40.0mm,width≤300mm |
Bar | Dia 8.0mm~Dia 32.0mm,length≤2000mm |
Dia 32.0mm~Dia 150.0mm,length:≤1000mm |
Condition: (With max tolerance) cold rolled,bright,hot rolled,burnished,hot forging,peeled,turned